I believe from reading online that the original ford babbitt formula was 86% tin 7% copper 7% antimony. I have the chance to purchase some babbitt bars that are 91% tin 4.5% copper 4.5 antimony, it's trade name is Adament and its made by the Magnolia Metals company. Has anyone ever used this? Is the mixture suitable for Model A engines? Thanks for any thoughts in advance.
George D is offline   Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Sponsored Links (Register now to hide all advertisements)


All times are GMT -5. The time now is 12:00 AM.