View Single Post
Old 01-29-2021, 06:18 PM   #27
OldGold360
Senior Member
 
Join Date: Nov 2020
Location: SW WA
Posts: 700
Default Re: 1936 P/U Metalshaping

I used .045” ER70s-2 filler rod. Gap between panels is tight. I push the puddle and not much filler rod is used. Being a small TIG weld, this allows me to flatten the weld and stretch the shrunk metal simultaneously. I’ve used smaller filler rod from my 110v mig wire, but the .045” is readily available and I get good results with it.

I’m still hoping to come up with some cab corners. I don’t have much time to work on my pickup so buying some would move me along faster. Thanks
OldGold360 is offline   Reply With Quote